subject
Chemistry, 22.03.2021 21:00 milkshakegrande101

An FCC iron-carbon alloy initially containing 0.20 wt% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0 wt%. If after 51 h the concentration of carbon is 0.35 wt% at a position 3.9 mm below the surface, determine the temperature at which the treatment was carried out. You will need to use data in the two tables below to solve this problem.

ansver
Answers: 2

Other questions on the subject: Chemistry

image
Chemistry, 21.06.2019 17:50, lm942747
Which best describes why nh4+ can form an ionic bond with cl-?
Answers: 3
image
Chemistry, 22.06.2019 01:40, janelisse199820
Non renewable resources like petroleum eventually
Answers: 2
image
Chemistry, 22.06.2019 13:00, netflixacc0107
Amixture with the same composition throughout is!
Answers: 1
image
Chemistry, 22.06.2019 21:50, isabel81ie
Given the data below for the reaction, 2 a + 2 b + 4 c => d + e + 3 f, the reaction is fill in the [ ] order in a, fill in the [ ] order in b, fill in the [ ] order in c and fill in the [ ] order overall. (use the words "first, second, third, fourth" to fill each blank)experimentinitial conc of a, mol/l initial conc of b, mol/l initial conc of c, mol/l initial rate, mol/l. s1 0.1 0.1 0.2 2 x 10-32 0.2 0.3 0.2 6 x 10-33 0.3 0.1 0.2 2 x 10-34 0.4 0.3 0.4 1.2 x 10-2
Answers: 2
You know the right answer?
An FCC iron-carbon alloy initially containing 0.20 wt% C is carburized at an elevated temperature an...